Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115 - Europe - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 12 cm³/10min ISO 1133
Temperature 260 °C -
Load 5 kg -
Thermal conductivity of melt 0.21 W/(m K) -
Spec. heat capacity of melt 2300 J/(kg K) -
Ejection temperature 142 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1370 MPa ISO 527
Yield stress 35 MPa ISO 527
Yield strain 5 % ISO 527
Stress at break 31 MPa ISO 527
Strain at break 50 % ISO 527
Flexural modulus 1520 MPa ISO 178
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 37 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 6 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm N kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, 4mm 36 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 4mm 10 kJ/m² ISO 180/1A
Rockwell hardness R 60 - ISO 2039-2
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, B 80 °C ISO 306
Vicat softening temperature, 120°C/h 50N 85 °C ISO 306
Coeff. of linear therm. expansion, parallel 70.7 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 101 E-6/K ISO 11359-1/-2
Other propertiesValueUnitTest Standard
Density 990 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 60 - 65 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 260 - 290 °C -
Mold temperature 40 - 60 °C -
Feed temperature 60 - 80 °C -
Zone 1 225 - 275 °C -
Zone 2 240 - 285 °C -
Zone 3 250 - 290 °C -
Diagrams
Viscosity-shear rate , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
Shearstress-shear rate , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
Specific volume-temperature (pvT) , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
Characteristics
Processing
Injection Molding
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.